Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL PPX™ Resin PPX7115 - Europe - (PPE+PP) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL PPX™ Resin PPX7115 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Noryl PPX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 12 cm³/10min ISO 1133
Température 260 °C -
Charge 5 kg -
Conductivité thermique du fondu 0.21 W/(m K) -
Chaleur spécifique du fondu 2300 J/(kg K) -
Température d'éjection 142 °C -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 1370 MPa ISO 527
Contrainte d'écoulement 35 MPa ISO 527
Déformation au seuil d'écoulement 5 % ISO 527
Contrainte à la rupture 31 MPa ISO 527
Déformation à la rupture 50 % ISO 527
Module de flexion 1520 MPa ISO 178
Résistance au choc Charpy, +23°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy, -30°C N kJ/m² ISO 179/1eU
Résistance au choc Charpy (entaillé), +23°C 37 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 6 kJ/m² ISO 179/1eA
Izod impact strength, +23°C, 4mm N kJ/m² ISO 180/1U
Izod impact strength, -30°C, 4mm N kJ/m² ISO 180/1U
Résistance au choc Izod (entaillé), +23°C, 4mm 36 kJ/m² ISO 180/1A
Résistance au choc Izod (entaillé), -30°C, 4mm 10 kJ/m² ISO 180/1A
Dureté Rockwell R 60 - ISO 2039-2
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, B 80 °C ISO 306
Température de ramolliss. Vicat, 120°C/h 50N 85 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 70.7 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 101 E-6/K ISO 11359-1/-2
Propriétés diversesValeurUnitéNorme du test
Masse volumique 990 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 60 - 65 °C -
Pré-séchage - temps 2 - 4 h -
L'humidité de traitement ≤0.02 % -
Température de la matière fondue 260 - 290 °C -
Température du moule 40 - 60 °C -
Température - Zone d'alimentation 60 - 80 °C -
Zone 1 225 - 275 °C -
Zone 2 240 - 285 °C -
Zone 3 250 - 290 °C -
Fonctions
Viscosité / Vitesse de cisaillement , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
Contrainte de cisaillement / Vit. de cisaillement , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
Volume spécifique (pvT) , NORYL PPX™  Resin PPX7115 - Europe, (PPE+PP), SABIC
Caractéristiques
Transformation
Moulage par injection
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com